The first three animations show the different growth modes of SrTiO3: ideal 2D layer by layer growth, 3D non-ideal growth and induced layer by layer growth by pulsed laser interval deposition. The fourth animation shows the deposition of an artificial YCuO2/BaCuO2 superlattice. The next animation shows the growth of SrRuO3 on TiO2 terminated SrTiO3. Finally, the last animation show our new PLD system, with in-situ AFM monitoring.